Revision as of 15:31, 15 December 2022 by Pyro>Pyroadmin (Skapade sidan med '== Fence-post prime == Källa: Eugene Yurek, https://www.amateurpyro.com/forums/topic/2676-fence-post-prime/ Composition 100g * Potassium Nitrate 65 * Charcoal Airfloat 12 * Sulfur 10 * Diatomaceous Earth 5 (Kiselgur)111 * Silicon, 325 mesh 5 * Charcoal, spruce, ball milled 3 Named for it's purported ability to light wet fence posts in a hurricane. The silicon burns and forms molten glass. I don't want to copy and paste the comments from passfire here but I'll try t...')
(diff) ← Older revision | Latest revision (diff) | Newer revision → (diff)
Jump to: navigation, search

Fence-post prime

Källa: Eugene Yurek, https://www.amateurpyro.com/forums/topic/2676-fence-post-prime/

Composition 100g

  • Potassium Nitrate 65
  • Charcoal Airfloat 12
  • Sulfur 10
  • Diatomaceous Earth 5 (Kiselgur)111
  • Silicon, 325 mesh 5
  • Charcoal, spruce, ball milled 3


Named for it's purported ability to light wet fence posts in a hurricane. The silicon burns and forms molten glass.

I don't want to copy and paste the comments from passfire here but I'll try to cover a few bases.. The DE makes this stuff pretty fluffy. Use about 1/3 less than you would with a regular prime. A layer 1-1.5mm thick is all you should ever need. If your stars are ridiculously difficult, up the silicon to no more than 10%.