Från Pyro
(Skapade sidan med '== Fence-post prime == Källa: Eugene Yurek, https://www.amateurpyro.com/forums/topic/2676-fence-post-prime/ Composition 100g * Potassium Nitrate 65 * Charcoal Airfloat 12 * Sulfur 10 * Diatomaceous Earth 5 (Kiselgur)111 * Silicon, 325 mesh 5 * Charcoal, spruce, ball milled 3 Named for it's purported ability to light wet fence posts in a hurricane. The silicon burns and forms molten glass. I don't want to copy and paste the comments from passfire here but I'll try t...') |
|||
| Rad 6: | Rad 6: | ||
* Charcoal Airfloat 12 | * Charcoal Airfloat 12 | ||
* Sulfur 10 | * Sulfur 10 | ||
* Diatomaceous Earth 5 (Kiselgur) | * Diatomaceous Earth 5 (Kiselgur) | ||
* Silicon, 325 mesh 5 | * Silicon, 325 mesh 5 | ||
* Charcoal, spruce, ball milled 3 | * Charcoal, spruce, ball milled 3 | ||
Nuvarande version från 8 februari 2023 kl. 11.23
Fence-post prime
Källa: Eugene Yurek, https://www.amateurpyro.com/forums/topic/2676-fence-post-prime/
Composition 100g
- Potassium Nitrate 65
- Charcoal Airfloat 12
- Sulfur 10
- Diatomaceous Earth 5 (Kiselgur)
- Silicon, 325 mesh 5
- Charcoal, spruce, ball milled 3
Named for it's purported ability to light wet fence posts in a hurricane. The silicon burns and forms molten glass.
I don't want to copy and paste the comments from passfire here but I'll try to cover a few bases.. The DE makes this stuff pretty fluffy. Use about 1/3 less than you would with a regular prime. A layer 1-1.5mm thick is all you should ever need. If your stars are ridiculously difficult, up the silicon to no more than 10%.